Alumina Grades Explained: 95% to 99.99% Purity and What Each Grade Buys

Alumina grades are named by their Al2O3 content by weight, and the six standard grades of alumina we produce run from 95% to 99.99%. Most designs only need to choose between a few of them, because a handful of steps in that range change what the part can do: 99% for high-voltage insulation and 1,500 °C service, 99.7% for strong acids and low RF loss, and 99.99% for contamination-sensitive semiconductor work.

Alumina ceramic grades here mean finished, sintered parts. All six also count as high alumina ceramic, a label that usually starts well below 95%. Alumina powders are sold under a separate set of names (calcined, tabular, fused, and others) that describe raw materials, not parts. Full grade-by-grade property tables sit on our alumina properties data hub.

Which Requirement Pushes You Up an Alumina Grade

Start at 95% and move up only when a specific requirement forces the change. Each step above 95% buys a defined set of improvements, not a general upgrade, so the useful question is which requirement your part cannot meet at the grade below.

Purity matters because of what fills the rest of the part. The last few percent are sintering aids, mostly SiO2, MgO, and CaO, added so the alumina powder fuses at a lower firing temperature. They leave a thin glass-like layer between the alumina grains, and that layer insulates less well, resists chemicals less well, and softens at a lower temperature than alumina itself. Less of it means a better part and a higher firing cost.

Read the table from top to bottom: each row lists only what that grade adds over the one before it.

GradeWhat it adds over the previous gradeTypical reason to choose itRelative cost
95%The economical baseline: a good low-voltage insulator and hard enough for most wear parts (volume resistivity >1013 Ω·cm, service to 1,350 °C, hardness HV 1410)General wear parts, low-voltage insulation, cost-driven jobsLowest
97%More heat headroom (service to 1,450 °C; bending strength rises from 292 to 311 MPa)Wear parts running hotter than 1,350 °CLow
99%The grade where alumina becomes a dependable high-voltage insulator (volume resistivity >1014 Ω·cm; dielectric loss halves to 2×10−4); also service to 1,500 °C, thermal conductivity of 14 to 21 W/m·K, and alkali mass loss halved to ≤0.1 mg/cm²High-voltage insulators, hybrid substrates, furnace parts between 1,350 and 1,500 °CModerate
99.5%The toughest of the six (fracture toughness 5.37 MPa·m½; bending strength 355 MPa), though its toughness is still a tenth or less of a typical steel's, so it resists chipping better but does not make alumina impact-proofVacuum feedthroughs, parts that take light knocks in handlingModerate
99.7%Much better acid resistance and the lowest signal loss (acid mass loss drops from ≤0.7 to ≤0.1 mg/cm²; dielectric loss 1×10−4)Strong-acid service; RF and microwave insulatorsHigher
99.99%The cleanest grade, for processes where impurities themselves are the problem (lowest impurity content; hardness HV 1660; thermal conductivity of 16 to 22 W/m·K)Semiconductor wafer contact, precision opticsHighest

Values are from our QC data; test conditions are listed on the data hub. Relative cost is a ranking, not a price; a quote also depends on geometry, quantity, and finishing.

White alumina ceramic plates and ivory alumina tubes and bars
White and ivory alumina ceramic parts; color varies with grade, and the 99% to 99.7% grades typically fire ivory.

In practice, three of these steps decide most specifications. The step to 99% is the insulation and temperature step: volume resistivity rises a full order of magnitude and continuous service reaches 1,500 °C, which is why 99% is the usual default for high-voltage parts, as our alumina ceramic insulator guide explains. The step to 99.7% is the acid-resistance step: acid mass loss falls seven-fold and dielectric loss reaches its lowest value. The step to 99.99% is about cleanliness; its strength gain over 99.7% is small (from 370 to 392 MPa). Published industry analysis notes that most alumina applications are well served below 99.9%, and grades above that exist to keep impurities out of a process.

What a higher grade does not buy

Two properties do not rise with purity, so climbing grades for them wastes money. Fracture toughness peaks at 99.5% (5.37 MPa·m½) and falls back to 4.3 to 4.4 above it. Dielectric strength reads 17.72 kV/mm at 99.7%, slightly below the 17.84 kV/mm of 95%. If a part chips under impact, a tougher material such as zirconia or zirconia toughened alumina is a better fix than a higher alumina grade. Higher grades are also harder, so they grind more slowly and cost more to machine; our guide to machining alumina covers the cost side.

How to Read an Alumina Grade on a Datasheet or Quote

Treat the percentage on a datasheet or quote as a label until you know whether it is a minimum or a nominal value, which of our grades it corresponds to, what the supplier's code means, and, for high-purity grades, which impurity limits apply.

Minimum versus nominal purity

Our alumina purity figures are minimums: 99.5% means at least 99.5% Al2O3 by weight. Ceramic datasheets do not all follow that convention. Some publish nominal or typical values instead, and the gap can be a full percentage point. One published 96% alumina, for example, is specified as a minimum of 95.0% Al2O3, typically 96%. When a drawing calls for 96%, ask which of those two numbers the quote guarantees.

Matching grades that are not on our list

Suppliers do not all offer the same alumina grades. Grades such as 94%, 96%, 99.6%, and 99.8% are common on other datasheets, while our standard range is 95%, 97%, 99%, 99.5%, 99.7%, and 99.99%. The safe rule is to match the minimum, not the label: choose the lowest standard grade whose minimum still meets the requirement.

Grade on the drawing or quote (minimum)Lowest standard grade that meets itNote
94%95%Meets the requirement with margin
96%97%96% is also available as a custom grade
98.5%99%
99.6%99.7%
99.8% or 99.9%99.99%If contamination set the grade, the impurity limits matter more than the percentage

If the figure on the original drawing is nominal, check its guaranteed minimum first. This table matches chemistry only. When the original grade was chosen for a property such as thermal conductivity, compare that property directly against the values on our data hub.

Supplier grade codes

Grade codes usually carry the purity in their digits, but not always. One supplier's AS999 is a 99.99% grade while its AG999 is 99.9%, and another supplier's FG-995, which reads like a 99.5% code, is nominally 98.5%. Read the purity line on the datasheet, not the code.

High-purity grades are specified in ppm

Above about 99.5%, the percentage alone stops being precise enough, because what matters is which impurities make up the last fraction of a percent. High-purity datasheets add limits on individual impurities in parts per million; one published 99.8% grade, for example, specifies soda and silica below 100 ppm. For a part that sits inside a semiconductor or analytical process, the impurity list is the real specification and the grade is shorthand.

How to Specify an Alumina Grade on a Drawing or RFQ

Write the grade as a minimum weight percentage, pair it with a property that can be checked on arrival, and state why the grade was chosen. A drawing that carries the following five items is hard to misread:

  • Purity as a minimum. "Alumina ceramic, ≥99.5% Al2O3 (wt%)" rather than "99.5% alumina".
  • A minimum density for the grade. For example, ≥3.90 g/cm³ for 99.5%, which gives incoming inspection a number to test.
  • Impurity limits in ppm, when contamination is the reason for the grade.
  • The duty that set the grade, such as temperature, voltage, frequency, or chemical exposure, so the supplier can flag a lower grade that still meets it.
  • A material certificate tied to the batch number, stating how the Al2O3 content was measured.

Once parts arrive, density by water displacement is the fastest check that a batch matches its grade, because each grade fires to a characteristic density, from 3.62 g/cm³ at 95% to 3.95 g/cm³ at 99.99%. Above 99%, neighboring grades differ by only 0.02 to 0.05 g/cm³, so density easily separates 95% from 99% but cannot tell 99.5% from 99.7% on its own; our guide to the density of alumina walks through the method. If you are unsure which grade fits, describe the operating conditions through our quote request form; our engineers recommend a grade free of charge and reply within 24 hours on business days.

Frequently Asked Questions

Check whether 96% is a minimum or a nominal value. If the drawing requires at least 96% Al2O3, 97% meets it and 95% does not. If 96% is nominal, the original part may only guarantee 95%. We can also produce 96% as a custom grade.

No. The N counts the nines, so 3N is 99.9% and 4N is 99.99%, a tenfold difference in allowable impurities. Datasheets sometimes blur the two, so confirm the actual percentage and, for semiconductor work, the ppm limits.

Usually, but not always. One supplier's AS999 is 99.99% while its AG999 is 99.9%, and another's FG-995 is nominally 98.5%. Check the purity line on the datasheet, not the code.

A material certificate tied to the batch number that states the Al2O3 content and how it was measured, such as XRF or ICP. A certificate listing only the grade name is a description, not a measurement. A density check gives a quick second opinion.

References

  1. CoorsTek, Advanced Alumina material properties datasheet
  2. Morgan Advanced Materials, alumina ceramic datasheets (GlobalSpec)
  3. Morgan Advanced Materials, AL998A high-purity alumina datasheet
  4. Ferrotec, alumina ceramic materials in multiple grades of purity
  5. Almatis, high-purity alumina article, American Ceramic Society Bulletin (April 2023)

Leave a Comment

Your email address will not be published. Required fields are marked *